Stone coating the possible problems in construction

by:Opal     2021-01-18
Stone coating as a kind of widely used in coating in our life, not only has beautiful effect, and has a strong performance. Today we make a brief introduction of stone coating problems need attention in construction process. Let xiao introduce you to.


corner crack of Yin and Yang: fluorine carbon spraying, Yin and Yang Angle can sometimes appear crack. As the Angle of Yin and Yang is the double, if the spray paint, drying in the process of the tension of two different directions at the same time affects on the Yin and Yang Angle of coating, easy to crack. Field solution: if it is found that cracks of Yin and Yang Angle, spray gun to spray once every half hour, until the cracks are covered; For a new spray Angle of Yin and Yang, pay special attention not to spray a thick, to adopt the method of multilayer thin spray, namely the surface dry again after spraying, spray gun to stay away from, faster movement speed. Don't in vertical injection of Yin and Yang, scattering, only is two faces, spray to sweep a mist on the verge of Yin and Yang Angle.


surface crack, the main reason for the great difference in temperature may be the weather lead to sudden drop in temperature, leading to the inner and outer drying speed is different, the surface cracks are formed when dry. The solution is to use small nozzle spray gun spraying thin layer, as far as possible to control the rate of each layer of dry, spray distance to slightly longer.


this is for KeBao building materials in construction stone coating of possible problems in the process of introduction, this article so far. If you are interested in stone paint, can focus on our website, thanks for reading!