Speak with authority, quality is trustworthy.

Do you know stone paint construction process and the matters needing attention?

by:Opal     2021-01-18
With the development of society and economy, our living standards are constantly improve, people on environmental protection, health and safety requirements more and more is also high. Stone coating as a kind of new wall materials, as a substitute for building exterior wall decoration protection, with its green and abundant species will have broad market space. Next, we will share stone coating construction technology and matters needing attention. Construction conditions (do not in damp or cold weather Temperature below 5 ℃, relative humidity higher than 85%) Construction, otherwise you won't achieve the desired coating effect. Maintenance time: 7 days / 25 ℃; In wet weather or temperature too low, should be appropriately extended time, in order to obtain ideal effect of paint film. 1 construction process. After the completion of the cement mortar of scraping, need maintenance more than 15 days, and completely dry. 2. With a batch of exterior wall elastic putty powder, and then the grid cloth. Blow dry completely, need external wall elastic one or two batch of scraping putty powder, make metope good flatness. 3. After drying and polishing, polishing and cleaning. Use ali master match seal primer to be completely sealed, no leakage. 4. Separation line construction: according to the height, width of the wall and design scheme of reasonable to partition and partition wall, draw off black paint, after being black paint is completely dry paste the cover of the high quality paper. 5. Before the construction to ensure uniform wall thickness, and spraying a layer of paint master ali granite. 6. In the coating after completely dry, spray paint, cover before construction, adjust the spray gun, to achieve the effect of construction before the template. 7. Paint, after the completion of construction shall be immediately clear marking masking paper, and repair the damaged area. 8. Paint and black paint on the line after fully dry, with matching paint spraying ali master stone paint. Note 1) Construction requirements: basic solid, solid, dry, level off, clean, no floating ash and oil; 2) Putty layer check: check base material before besmear brushs paint putty and ph value of water content, water content of 10% or less, the ph value of 10 or less; 3) Environmental requirements: temperature should not be lower than 5 ℃, humidity should be lower than 85%; Avoid wind, rain and snow weather; 4) Primers must be uniform coating, at the grass-roots level must be completely closed. Prohibit direct adjustment primer black instead of lacquer painting line. 5) Stir well before use, special circumstances when diluted with water, add water should be controlled within 5%. 6) Surface drying or 4 h ( The environment temperature 25 ℃) At least 24 h, recoat time ( The environment temperature 25 ℃) 7) Every batch of products after arrived at the scene, should be small sample test, and color confirmation. 8) In the same on metope, please use the same product, in order to prevent the batch off color keep the same thickness of pressure equipment, construction method, construction, etc. In the same on metope, prevent defects such as crack, seepage and color difference, the frost. 9) Clean with clear water used tools. The above is KeBao paint a bit assembly. I want to share stone paint construction process and the matters needing attention. In construction process, you must master the above skills, to build a more beautiful exterior. I hope this is helpful to you. Interested in stone coating friend can read more about the stone coating the effect factor of really stone paint have? 2019 KeBao paint tech-oriented explanation 'of information.
Chat Online
Chat Online
Chat Online inputting...
Sign in with: