Speak with authority, quality is trustworthy.

Really stone paint construction technology and introduced in detail

by:Opal     2021-01-25
Really stone paint has the waterproof, never fade, not aging, flame retardant, heat insulation, weather resistance and other advantages, is the preferred high-end decorative surface building insulation. KeBaoZhen stone paint, however, to remind us: the three points, seven points, high quality really stone paint should be combined with scientific construction technology, after the completion of the wall outside facing can achieve the best decoration effect, the organic combination of appearance and natural environment, to show the effect of all kinds of stone material and ceramic tile. Today, the side xiao will introduce to you detailed really stone paint construction technology and equipment. Really stone paint construction equipment requirements: ( 1) Air compressor: more than 5 units, air volume is enough, at least three duct, can meet the requirements of three or more persons at the same time the construction. ( 2) The tank gun: capacity of 500 ml, diameter of 1. More than 3 mm, capacity cannot too big, otherwise is too heavy, not convenient operation, small calibre construction speed is slow, time limit for a project may be delayed, not suitable for large scale construction. ( 3) Really stone paint spray gun: single gun, double guns, three guns, etc. According to the different color choose single gun, double gun and three shots, to adapt to the different construction technology, spray effect is more ideal. ( 4) All kinds of diameter of nozzle: 4 mm, 5 mm, 6 mm, 8 mm, etc. According to the requirement of the template to select different nozzle. The smaller the diameter is, the smoother the spraying effect is even, the greater the size, the larger the dot, AoTuGan stronger. Really stone paint construction technology: 1. Foundation treatment, before foundation wall needs certain maintenance cycle. Blow be bored with child before, at the grass-roots level shall be completely eliminated the loose, peeling, empty drum and powder, and then remove dust, grease and other contaminants. With exterior wall putty to repair the wall and local leveling for the first time. With putty or sealant filled large holes and cracks. Be bored with child after drying, partial grinding metope, then use the whole batch of putty erased at the grass-roots level. Be bored with child after completely dry, grinding smooth at the grass-roots level. Because really stone paint has a certain thickness of thin plate coating high than the flatness requirement of the grassroots. 2, besmear to brush seal primer, be bored with child after completely dry, besmear again brush seal primer. Usually do not need to use additional seal primer diluent dilution. Its purpose is to clean and increase the intensity of the at the grass-roots level and bond strength of coating. Usually, use roller structure, can also use the spray structure. 3. Coating solid primer coating color primer purpose is to make the base material with the same color. The present invention can effectively avoid the shading phenomenon caused by really stone paint transparent coating, can also reduce the dosage of really stone paint, color uniform good decorative effect. Grassroots coloring material mainly has the good adhesion, durability and water resistance of external scumble emulsioni paint. Based on determining the color of the color of natural stone material or sample board, make the paint color as close as possible to the real stone the color of the paint itself. At the bottom of the coating must be uniform coating, position shall not be leakage or seepage. Usually, it will be used twice. In order to achieve stone adornment effect, at the same time, easy operation, can be segmented spraying really stone paint, the selected color of paint can be coated on the segment joint, spraying area, block seam should be completely blocked or scratching. 4. When spraying 'really stone paint' generally don't need water, can be adjusted by adding a small amount of water when necessary. However, control product structure should be paid attention to when spraying the consistency of the viscosity, air pressure, nozzle size and distance must be strictly consistent. When the weather is windy weather, should stop the construction. Really stone paint construction is very difficult. If the control is bad, the coating is easy to cause local flower. When spraying really stone paint, therefore, be careful not to on the metope of the spray gun discharge and collection. In addition, the spray gun movement speed should be uniform. For each spraying the edge of the range, in order to protect the decorative surface, increase the luster, improve resistance to pollution, enhance the overall decoration effect, after spraying coating, the coating surface, spray varnish. (after really stone paint dry completely Usually in the sunny days to save at least 3 days) , you can spray paint. In the process of construction, add a little thinner. Should pay attention to keep the viscosity, pressure and nozzle size are consistent, and to prevent sagging. Above is edge xiao summary for everyone really stone paint construction technology and introduced in detail. More consulting about really stone paint, please contact KeBao or reading the common problems and solutions of really stone paint '.
Chat Online
Chat Online
Chat Online inputting...
Sign in with: