Speak with authority, quality is trustworthy.

Really stone paint construction technology of technical indicators have?

by:Opal     2021-01-25
In recent years, really stone paint has become more and more popular. Exterior wall adornment basically is to use really stone paint finish. Really stone paint construction not only requires really stone paint quality reach the standard, also requires a high standard of facilities and strict construction technology. Although manufacturer of paint quality is good, but if lack of experience, low quality, construction personnel don't know or don't understand the performance of different manufacturers really stone paint, can cause all sorts of problems. Next, we will share with you really stone paint construction technology of technical indicators. Construction equipment and really stone paint requirements: ( 1) Air compressor: more than 5 units, air volume is enough, at least three duct, can meet the requirements of three or more persons at the same time the construction. ( 2) The tank gun: capacity of 500 ml, diameter of 1. More than 3 mm, capacity cannot too big, otherwise is too heavy, not convenient operation, small calibre construction speed is slow, time limit for a project may be delayed, not suitable for large scale construction. ( 3) Really stone paint spray gun: single gun, double guns, three guns, etc. According to the different color choose single gun, double gun and three shots, to adapt to the different construction technology, spray effect is more ideal. ( 4) All kinds of diameter of nozzle: 4 mm, 5 mm, 6 mm, 8 mm, etc. According to the requirement of the template to select different nozzle. The smaller the diameter is, the smoother the spraying effect is even, the greater the size, the larger the dot, AoTuGan stronger. 'Really stone paint' construction technology: 12 hours after 24 hours, burnish spray bottom oil - twice 2 - spraying really stone paint 3mm- Spraying the surface oil two indicators: (really stone paint construction technology 1) At the end of spraying oil: use for 4 - pressure 7 kg/cm2 of tank gun, construction temperature of not less than 10 degrees Celsius, spraying twice, 2 hours, about 30 microns thickness, normal temperature drying for 12 hours. ( 2) Spraying really stone paint: use really stone paint spray gun, air pressure control in 4 - 7 kg/cm2, construction temperature above 10 ℃, the thickness of about 2 - 3 mm. If you need two or three layers, for 2 hours, dry after 24 hours can be polished. ( 3) Polishing: with a 400 - 600 mesh sandpaper gently raised sand grinding really stone paint surface. Note do not force is too large, or film will damage, the bottom will become loose. In serious cases, the adhesion is very poor, really stone paint will fall off. ( 4) Coating on the surface of oil: use for 4 - pressure 7 kg/cm2 of tank gun, construction temperature shall be not less than 10 ℃. Spraying twice, 2 hours, the thickness of about 30 microns. It takes seven days to completely dry. Above is KeBao building materials edit Shared really stone paint construction process technical indicators. Really stone paint construction not only requires really stone paint quality reach the standard, also requires a high standard of facilities and strict construction technology. I hope this is helpful to everyone. Interested in really stone paint friend can read more about really stone paint 'really stone paint when construction: why do you want to spray finish? 'The information.
Chat Online
Chat Online
Chat Online inputting...
Sign in with: